BegoCer® G
BEGO · #61097
Automatically collected from eshop.bego.com
Are you the manufacturer?Send us your data
Gold-Basis-Aufbrennlegierung
Product Information
| Manufacturer | BEGO |
|---|---|
| Coefficient of thermal expansion (CTE) | 13,2 10ˉ⁶ Kˉ¹ |
| Density | 13.8 g/cm³ |
| Hardness | 195 HV10 |
| Temperature | 1450 °C |
| Elongation at break | 16 % |
| Content/quantity | 1 g |
| Yield strength | 430 MPa |
| Composition | Au 51,5 · Pd 38,4 · In 8,7 · Ga 1,3 · Ru |
| Elasticity Modulus | 153 GPa |