PlatinLloyd® KF

BEGO · #61025

Automatically collected from eshop.bego.com

Are you the manufacturer?Send us your data

Gold-Basis-Aufbrennlegierung für LFC-Massen

Product Information

ManufacturerBEGO
Coefficient of thermal expansion (CTE)15,3 10ˉ⁶ Kˉ¹
Density15.3 g/cm³
Hardness245 HV10
Temperature1200 °C
Elongation at break4 %
Content/quantity1 g
Yield strength560 MPa
CompositionAu 72,8 · Ag 16,1 · Pd 5,7 · Zn 3,0 · Pt 2,0 · Ir · Mn · Rh
Elasticity Modulus109 GPa