Albabond® A - for C&B 1172 8000

Kulzer · #1172 8000

Collecté automatiquement depuis kulzer.de

Vous êtes le fabricant ?Transmettez vos données

Texte du fabricant en anglais

Benefits

  • Containing silver
  • Suitable for ceramic veneering (e.g. HeraCeram Saphir)
  • Many years of user experience

Indications

  • Crowns
  • Bridges
  • Milling procedures
  • Implants

Specifications

Pd-based ceramic bonding alloy acc. to EN ISO 9693-1 and 22674, white s= self-hardening alloy after slow cooling in the mould v= Condition after hardening k= Bonding alloy: condition after ceramic firing

Contraindications

In case of hypersensitivity (allergies) to one of the constituents of the alloy.

Side effects

In individual cases hypersensitivity reactions (allergies) or electrochemically conditioned, local malsensations were reported.

Interactions with other dental alloys

With approximal or antagonist contact with dentures of different alloys galvanic effects may occur. Other materials must be used instead if contact with other alloys causes persistent local paraesthesia on an electrochemical basis.

Remarks

A = A stable framework design with reinforced connections with a cross-section of 8 –10 mm2 is required for long span bridges and suprastructures. Additionally, the frameworks need to be hardened. B = Depending on the copper and/or silver content, in some cases discoloration of double crowns may result after short period of wearing. C = In exceptional cases these alloys can also be used for traditional telescopic crowns with parallel walls and for the bar casting technique provided that cross-sections for crown walls, approximal areas, bars and laser welded joints are particularly thick and the alloy is hardened subsequently. No indication for conical crowns and shear distributors. D = Type classification acc. EN ISO 22674

Informations produit

FabricantKulzer
Coefficient de dilatation thermique (CDT)14.7
Couleurblanc
TeinteDark white
Densité11.4 g/cm³
NormeEN ISO 9693-1 and 22674
Type d'alliagePd-based ceramic bonding alloy
IndicationCrowns Bridges Milling technique Implant restorations
Température1440 °C
Plage de fusionSolidus 1165 °C Liquidus 1285 °C
Classification4 (s/v/k)