High-gold-content ceramic bonding alloy acc. to EN ISO 9693-1 and 22674, yellow colour
Benefits
- Gold content 86.6 mass% (precious-metal content 98 mass%)
- high corrosion-resistant
- free from Pd, Ag and Cu
- easily polished and milled
- Suitable for ceramic veneering (e.g. HeraCeram Saphir)
- Many years of user experience
Indications
- Single crowns
- Bridges of any span length
- Implant restorations(A)
- Milling technique
Contraindications
In case of hypersensitivity (allergies) to one of the constituents of the alloy.
Side effects
In individual cases hypersensitivity reactions (allergies) or electrochemically conditioned, local malsensations were reported.
Interactions with other dental alloys
With approximal or antagonist contact with dentures of different alloys galvanic effects may occur. Other materials must be used instead if contact with other alloys causes persistent local paraesthesia on an electrochemical basis.
Informations produit
| Fabricant | Kulzer |
|---|---|
| Coefficient de dilatation thermique (CDT) | 14.5 |
| Teinte | Jaune |
| Indication | Crowns Bridges Milling technique Implant restorations(A) |
| Température | 1290 °C |
| Teneur en or | 86.6 mass% |
| Temps de durcissement | 15 min. |