Starbond CoS
S&S Scheftner · #133000
Collecté automatiquement depuis scheftner.dental
Vous êtes le fabricant ?Transmettez vos données
Texte du fabricant en anglais
Starbond CoS
CoCrWMo bonding alloy for conventional, high-fusing (low expansion) ceramics. Free of nickel, lead, beryllium and cadmium. Type 5 pursuant to DIN EN ISO 22674.
- High degree of purity
- Biocompatible and extremly corrosion resistant
Advantages for Dental Technicians:
- Wide range of indications
- System-free working due to very good alloy properties
- Pleasant polishing properties and easy finishing due to low hardness of 280 HV10
- A CTE of 14.0 enables flexibility in ceramic selection and safe veneering
- No cooling phase required, depending on the ceramics
- Excellent metal-ceramic bonding, even without bonder
- An oxidation firing can be omitted
- Optimal conditions for laser welding
- Application flexibility and easy melting, no sparking
Composition:
Co: 59%
Cr: 25%
W: 9.5%
Mo: 3.5%
Si: 1%
C,Fe,Mn,N: <1%
Technical properties:
Proof stress (Rp 0.2): 650MPa
Ultimate tensile strength: 910MPa
Elongation: 8%
Elastic modulus: 200GPa
Vickers hardness: 280 HV 10
Density: 8.8g/cm³
Melting range: 1305 - 1400°C
Preheating temperature: 850 - 950°C
Casting temperature: 1500 - 1550°C
CTE (20-600°C): 14.0 x 10⁻⁶K⁻¹
Laser weldable: Yes
Type (DIN EN ISO 22674): 5
Trade unit:
1000g - Ref. 133000 250g - Ref. 133250
Informations produit
| Fabricant | S&S Scheftner |
|---|---|
| Densité | 8,8g/cm³ |
| Dureté | 280 HV 10 |
| Elongation | 8% |
| Application | Conventional, high-fusing (low expansion) ceramics |
| Température | 1500 - 1550°C |
| Allongement à la rupture | 8% |
| Plage de fusion | 1305 - 1400°C |
| Résistance à la traction | 910MPa |
| Elasticity Modulus | 200GPa |
| Température de préchauffage | 850 - 950°C |