Starbond CoS Powder
S&S Scheftner
Collecté automatiquement depuis scheftner.dental
Vous êtes le fabricant ?Transmettez vos données
Texte du fabricant en anglais
Starbond CoS Powder
Starbond CoS Powder is based on the proven dental bonding alloy Starbond CoS. The user can thus continue to work in a system with the same alloy components and the same composition, as well as the same positive processing characteristics.
The manufacturing process of the powder ensures the best possible flowability.
- No cooling phase required, depending on ceramics
- Excellent veneering
- A CTE of 14.4 permits great flexibility in ceramic selection
- Biocompatible
- Extremely corrosion resistance
- CE certified
Composition in percent by mass:
- Co: 59%
- Cr: 25%
- W: 9.5%
- Mo: 3.5%
- Si: 1%
- C, Fe, Mn, N: <1%
Technical properties:
- Proof stress (Rp 0.2): 720-1130 MPa
- Ultimate tensile strength: 990-1250 MPa
- Elongation: 2-10%
- Elastic modulus: 195-200 GPa
- Vickers hardness: 345-490 HV 10
- Density: 8.8 g/cm³
- Melting range: 1305-1400°C
- CTE (20-600°C): 14.4 x 10⁻⁶K⁻¹
- Laser weldable: Yes
- Type (DIN EN ISO 22674): 5
Informations produit
| Fabricant | S&S Scheftner |
|---|---|
| Densité | 8,8 g/cm³ |
| Dureté | 345-490 HV 10 |
| Type d'alliage | CoCr |
| Elongation | 2-10% |
| Allongement à la rupture | 2-10% |
| Plage de fusion | 1305-1400°C |
| Résistance à la traction | 990-1250 MPa |
| Elasticity Modulus | 195-200 GPa |